General - How to repair broken parts

ID: 146858

Description: Cyan acrylate or super glue alone may join...

Steps:

  1. You need cyan acrylate glue and glass sand with a particle size of 0.05 to 0.5 mm.
  2. Glass sand has the advantage that it is alkaline and therefore the glue cures rapidly.
  3. Step image
  4. To speed up curing activator helps a lot.
  5. Step image
  6. Make sure, the glueing areas a free of dirt, dust and grease.
  7. Step image Step image
  8. Add a little glue onto the damage area.
  9. Step image
  10. Scatter glass sand onto the glue and wait until it's cured. Eventually spray a little activator onto it.
  11. Step image
  12. Add more glue
  13. Step image
  14. Again scatter glass sand onto the glue. Alternating add glass sand and glue until the desired layer thickness has reached.
  15. Step image
  16. As soon as the desired layer thickness has reached and the glue is cured, the parts may be strained.
  17. Step image Step image