Steps:

  1. Start by cutting and removing any current filament that is loaded inside the nozzle. Then heat the nozzle by pressing the nozzle temperature icon, a popup should appear asking you how hot you would like the nozzle. Heat up to 230 degrees or higher.
  2. The heat bed does not need to be heat up.
  3. Step image
  4. Removing the PTFE tube is simply pulling it off.
  5. Step image
  6. Grab unused filament and slowly push it down the nozzle.
  7. Once you think you have pushed far enough(Ideally untill filament starts to ooze out of the nozzle) yank it out with a swift movement to grab any dust
  8. Do this as many times as desired(5-7 times is ideal, but for more thorough cleaning, 9-12 or more is needed)
  9. Step image
  10. Put back the PTFE tube, and done.
  11. Step image